Please use this identifier to cite or link to this item: https://has.hcu.ac.th/jspui/handle/123456789/3676
Title: Comparison of thermoelectric properties of flexible bismuth telluride thin films deposited via DC and RF magnetron sputtering
Authors: Piya Jitthamapirom
Pornsiri Wanarattikan
Pilaipon Nuthongkum
Rachsak Sakdanuphab
Aparporn Sakulkalavek
ปิยะ จิตธรรมมาภิรมย์
พรสิริ วนรัฐิกาล
พิไลพร หนูทองคํา
ราชศักดิ์ ศักดานุภาพ
อาภาภรณ์ สกุลการะเวก
King Mongkut’s Institute of Technology Ladkrabang. College of Advanced Manufacturing Innovation
Huachiew Chalermprakiet University. Faculty of Science and Technology
King Mongkut's Institute of Technology Ladkrabang. Faculty of Science
King Mongkut’s Institute of Technology Ladkrabang. College of Advanced Manufacturing Innovation
King Mongkut's Institute of Technology Ladkrabang. Faculty of Science
Keywords: Thin films
ฟิล์มบาง
Bismuth telluride
บิสมัทเทลลูไรด์
Condensed Matter Physics
ฟิสิกส์ของสสารควบแน่น
Thermoelectric materials
วัสดุเทอร์โมอิเล็กทริก
Magnetron sputtering
แมกนีตรอนสปัตเตอริง
Sputtering (Physics)
สปัตเตอริง (ฟิสิกส์)
Issue Date: 2019
Citation: Ferroelectrics, 552, 1 : 64-72
Abstract: Bi2Te3 thin films were deposited onto polyamide sheets with direct current (DC) or radio frequency (RF) magnetron sputtering techniques. The films were prepared using a Bi2Te3 target at a varying preheating temperature from 150 to 350 ° C. It was observed that the type of plasma excitation and pre-heating temperature can significantly change the composition, preferred orientation, crystallinity, and thermoelectric properties of the films. The pre-heat treatment significantly affected the non-stoichiometric composition. In addition, it was shown that crystallinity and (0 0 l) planes were enhanced in the DC sputtered coatings at a high pre-heating temperature. The maximum power factor of 3.5 10-3 W/m K2 at 285 °C was obtained for the films deposited using DC magnetron sputtering and a preheating temperature of 350 °C. The carrier concentration and mobility of the film were 5.40 1020 cm-3 and 13.04 cm2 /V s, respectively. Compared with an ordinary Bi2Te3 film, the power factor of such film has been greatly increased. The results indicated that DC magnetron sputtering can enhance the (0 0/) plane orientation in the Bi2Te3 film.
Description: สามารถเข้าถึงบทความฉบับเต็ม (Full Text) ได้ที่: https://colab.ws/articles/10.1080%2F00150193.2019.1653083
URI: https://has.hcu.ac.th/jspui/handle/123456789/3676
Appears in Collections:Science and Technology - Artical Journals

Files in This Item:
File Description SizeFormat 
Comparison-of-thermoelectric-properties-of-flexible-bismuth-telluride-thin-films.pdf65.26 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.